ДОНЕЦКИЙ ГОСУДАРСТВЕИНЫЙ ТЕХНИЧЕСКИЙ УНИВЕРСИТЕТ
ПРОГРЕССИВНЫЕ ТЕХНОЛОГИИ И СИСТЕМЫ МАШИНОСТРОЕНИЯ Международный сборник научных трудов ВЫПУСК 8


ДОНЕЦК-1999        
EC0L0GICAL PRODUCTION OF NEW CAST ALLOYS USING WASTE VOLATILE ELEMENTS(NITROGЕN ETC.) UNDER PRESSURE Kolev  Bogomil Velikov (Institute of Metal Science, BAS, Sofia, Bulgaria), E-mail:b.v.kolev@abv.bg It is been the custom In think that stable nitrogen concentrations can be ob- tained only in steels of the stainless type. Due to this, there is no informationthe influence of the main components in the system Fe-Cr-Mn-C on the cristization and maintaining of hyper-equilibnum nitrogen quantities in relation atmospheric conditions in castings of alloys with under 12-14% Cr The work introduces some technological results from the investigations o influence of C, C.r, Mn, etc. on the absorption and maintaing of hyper equilibrium nitrogen concentrations in relation to the atmospheric conditions in casting allays of the system Fe-Cr-Mn-C containing under 12-14% Cr and (ru.il$M under pressure. 1. Introduction The Fe-Cr-Mn-C-N system represents a particular interest for productionof founded and plastic deformation treated products that have to mach requirements of high mechanic indicators-wear resistance, corrosion resistence, non magnetivity, etc. The expensive and scarce Ni may be siuK-wdM substituted for N and Mn coating in the classical austenite alloys on Fe-C sistem. The research in C[l-5], Mn[3-4,6,12] and Cr[12,14-15] influence on solubility in alloys of Fe-C basis are usually relegated to rather  concentrations, to pure alloys or to bi-component systems. As far as N soludifi in Cr alloyed steels is concerned, the usually published data iclci *« I concentrations above 15-18% under standard conditions-temperatuu- I"1"*! and N pressure l.lO"^Pa. In [7] has been indicated that N solubiliu m i 4 steels under the above mentioned conditions is approximately 1/1 CM > p.m «fl Cr content in Cr-Mn steels-1/75 part and in Cr-Ni-Mn steels amoiuil". i "• •»■ 1/58 part of the content of Cr and from 1/72 to 1/92 part of the whole ■■".•••nf Cr+Mn. Another essentional problem in the process of N-coating of ihc minM the preservation of N in the process of crystalization and the prevention


Тагове:   украйна,   доклад,   Богомил,


Гласувай:
0



Няма коментари
Вашето мнение
За да оставите коментар, моля влезте с вашето потребителско име и парола.
Търсене

За този блог
Автор: bogomil
Категория: Други
Прочетен: 2030166
Постинги: 452
Коментари: 1153
Гласове: 1970
Календар
«  Април, 2024  
ПВСЧПСН
1234567
891011121314
15161718192021
22232425262728
2930